http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I642800-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_40a53034e1a3f706ea1e49130cbfdef7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-851 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-34 |
filingDate | 2017-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a1e685b57996ee6eadebba9511ab136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8954e701ee68a59a2bb9fbdeb2ec9001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a9dd371b45122f70d2cf677c0ffba6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_556402ae401832eb6ab2cff2b9bba8fa |
publicationDate | 2018-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I642800-B |
titleOfInvention | Cobalt-platinum-ruthenium-based sputtering target, preparation method thereof and magnetic recording layer |
abstract | The present invention provides a cobalt platinum rhodium sputtering target, a preparation method thereof and a magnetic recording layer. The cobalt platinum ruthenium sputter target and the magnetic recording layer have a similar composition, comprising cobalt, platinum and rhodium, the ruthenium content being greater than or equal to 0.2 atomic percent and less than or equal to 3.5 atomic percent, and the platinum content relative to cobalt and The ratio of the content of platinum is greater than or equal to 0.15 and less than or equal to 0.3. By controlling the composition of the cobalt-platinum-ruthenium-based sputtering target and the magnetic recording layer, it is possible to improve the saturation magnetization amount, the magnetocrystalline anisotropy constant, and the grain size uniformity of the magnetic recording layer, thereby making the magnetic recording layer-containing layer The magnetic recording medium has a high magnetic recording density and a good recording quality. |