http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I617585-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2755c806997dfe83a65d0368c30fda8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2baf849d216e689ecc40ccc931a7a7bc |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133726 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K19-542 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F290-148 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F283-124 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F290-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133711 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133788 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F290-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 |
filingDate | 2013-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ca988a9e11092163b26b06f5c0bdd4f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e9163f9be9030577087105b7cc912a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1b18d3a587ec189988478eba15aacf3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02ac9f35e87e7683e8347a9fb4c7469a |
publicationDate | 2018-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I617585-B |
titleOfInvention | Manufacturing method of liquid crystal alignment film, liquid crystal alignment film, liquid crystal display element, polymer and liquid crystal alignment agent |
abstract | The present invention provides a liquid crystal alignment film and a liquid crystal display element by a method for manufacturing a liquid crystal alignment film with high efficiency using light.nn n n A polymer is obtained by polymerizing a polysiloxane with a monomer having a liquid crystallinity and a photosensitive group and a radical polymerizable group, thereby preparing a liquid crystal alignment agent. After the liquid crystal alignment agent obtains the side chain type polymer film (1), the polarized ultraviolet rays are irradiated for alignment treatment, and then the side chain (2) of the side chain type polymer film (1) is re-aligned by heating. Next, it is heated at a high temperature to fix the re-alignment state to produce a liquid crystal alignment film. The heating temperature for realignment is, for example, 200 ° C. or lower, and the temperature is 10 ° C. higher than the lower limit of the temperature range in which the side chain polymer film (1) exhibits liquid crystallinity, and 10 ° C. lower than the upper limit. A liquid crystal display element was manufactured using the obtained liquid crystal alignment film. |