http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I274047-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3dc860e6deefd033750b3ad89d0e6430 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-089 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-093 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-095 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-085 |
filingDate | 2003-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78a34b0c3be1c285dbdeaec8ceb9292d |
publicationDate | 2007-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I274047-B |
titleOfInvention | A glass for metal or alloy sealing |
abstract | In order to provide a glass which can be sealed with metal or alloy has a linear coefficient of thermal expansion matched with metal or alloy, a low number of producing bubbles and a low liquidus temperature. The sealing glass which consists, by mole, of 70.0%-80.0% SiO2, 0.0%-4.0% Al2O3, 12.0%-19.0% B2O3, 0.0%-4.0% Li2O, 0.0%-6.0% Na2O, 0.0%-8.0% K2O, Li2O+Na2O+K2O 3.0%-11.0%, 0.0%-2.0% MgO, 0.0%-2.0% CaO, 0.0%-2.0% SrO, 0.0%-2.0% BaO, MgO+CaO+SrO+BaO 0.0%-4.0%, 0.0%-2.0% ZnO, 0.0%-1.0% As2O3, 0.0%-1.0% CeO2, As2O3+CeO2 0.05%-1.0%. |
priorityDate | 2003-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.