http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I266780-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9f26cd77b1fd6f8bd8a20b78c1126fa6 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2331-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2009-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C61-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D7-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D71-08 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D71-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C61-00 |
filingDate | 2004-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2006-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-I266780-B |
titleOfInvention | B29k 105/02 200601 a x htw b29l 7/00 200601 a x htw |
abstract | A shrinkable film having excellent dimensional stability at 60 DEG C and satisfactory shrinkability at 100 DEG C and 120 DEG C. It is a low-temperature shrinkable film comprising at least one layer which comprises at least one ethylene/alpha-olefin copolymer (A) having a density of 0.870 to 0.920 g/cm<3> and at least one ethylene copolymer (B) which, in the second melting behavior in an examination with a differential scanning calorimeter, has the main peak at a temperature lower than 110 DEG C, wherein the ethylene/alpha-olefin copolymer (A), in the second melting behavior in an examination with a differential scanning calorimeter, gives a curve in which the proportion of the quantity of heat of fusion in the temperature range up to 100 DEG C to the total quantity of heat of fusion is 50 to 100%, and the film, in the second melting behavior in an examination with a differential scanning calorimeter, gives a curve in which the proportion of the quantity of heat of fusion in the temperature range up to 100 DEG C to the total quantity of heat of fusion is 60 to 100%, the average of the degree of machine-direction thermal shrinkage and that of transverse-direction thermal shrinkage of the film being 0 to 15% at 60 DEG C, 50% or higher at 100 DEG C, and 70% or higher at 120 DEG C. |