Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8475d4116549bb1d8a2dd1f15d7d3dbf |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-886 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-0234 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8807 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8835 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 |
filingDate |
2001-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2004-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce4e475f7242dfc7b4e20daa36f4c28d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_244ea9173613742ed90f75c88049ba9a |
publicationDate |
2004-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-583091-B |
titleOfInvention |
Gas diffusion electrode manufacture and MEA fabrication |
abstract |
A method for producing a gas diffusion electrode in which a slurry of carbon black, alcohol, water and a tetrafluoroethylene emulsion is applied as a layer a non-Teflonized carbon cloth substrate, which is then heated to remove water. The dried coated carbon cloth is then rolled followed by heating to remove wetting agents present in the tetrafluoroethylene emulsion. The coated carbon cloth is then cooled and rolled again to produce the final end product. |
priorityDate |
2001-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |