Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-3045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-3063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-65912 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-222 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-346 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 |
filingDate |
2020-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11b6bac084a77732dfb5d748990acda5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b9e35ee99d5ba6dee3d1199039cbcf6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7de0840988bb66b1e2c189d11927fc68 |
publicationDate |
2021-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-202124560-A |
titleOfInvention |
Resin composition, molded body, sheet, toy, daily miscellaneous goods, and electronic device frame |
abstract |
The problem to be solved by the present invention is to provide a resin composition and a molded body that have high stress relaxation properties and vibration absorption properties at room temperature and suppress surface stickiness. A resin composition (X), containing 10 parts by mass to 50 parts by mass of thermoplastic resin (A) and 50 parts by mass to 90 parts by mass of inorganic substance (B), and in the temperature range of -40°C to 150°C, with 10 rad The tanδ peak temperature obtained by the dynamic viscoelasticity measurement at a frequency of /s (1.6 Hz) is 0°C or more and 60°C or less, and the tanδ peak value is 0.8 or more and 5.0 or less. |