http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-202109097-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate | 2020-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_422eba9f0baf2d841709ec07aa04000b |
publicationDate | 2021-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-202109097-A |
titleOfInvention | Polarizing plate with pressure-sensitive adhesive layer |
abstract | An objective of this invention is to provide a polarizing plate with pressure-sensitive adhesive layer including a pressure-sensitive adhesive layer containing an antistatic agent, which is hardly peeled off even when subjected to a physical shock. A polarizing plate with pressure-sensitive adhesive layer of this invention contains a polarizing plate, and a pressure-sensitive adhesive layer laminated and in contact with the polarizing plate, which has four sides and four corners, wherein at least one corner is a rounded corner having a radius of curvature of 1.0 mm or more, and the pressure-sensitive adhesive layer contains an antistatic agent. If the resistance values of the surface of the pressure-sensitive adhesive layer on the side opposite to the polarizing plate side before and after being held at a temperature of 85 DEG C for 100 hours are set to be R1 [[Omega]/□] and R2 [[Omega]/□], respectively, the change rate [Delta]R [%] calculated by formula (3) satisfies the relationship of formula (1). [Delta]R=[(R2-R1)/R1]*100 (3) [Delta]R ≥ 25 (1). |
priorityDate | 2019-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |