Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_962adbf7d50e742218f3d536a63df612 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2433-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-312 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-6836 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-35 |
filingDate |
2020-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59906fb06d817c15dfe03e99360575d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf1db307d863977de9439a0a06fa4a0d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed860187e9669ebe5b31401e7c5272c2 |
publicationDate |
2021-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-202104482-A |
titleOfInvention |
Adhesive sheet and laminate |
abstract |
[Problem] It is possible to provide an adhesive sheet with excellent handleability even in the case of heat treatment. [Solution] An adhesive sheet comprising at least an adhesive layer, wherein the adhesive sheet is used to fix the workpiece on the substrate through the adhesive layer during the process and remove the workpiece from the adhesive after the process is completed The use of layer peeling, and the adhesive layer is composed of an active energy ray-curable adhesive, and the initial adhesive force of the adhesive sheet is set to F 0 , and it will be heated at 150° C. for 30 minutes and then further irradiated. When the adhesive force of the adhesive sheet after the energy beam is F 2 , the ratio of the adhesive force F 2 to the initial adhesive force F 0 (F 2 /F 0 ) is 0.3 or less. |