http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-202104088-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_06ed0f0cc4866156f05b170d95d7d151 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1253 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G25-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-1016 |
filingDate | 2020-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2a21237e2ad00e0b8103a1ab1f1e03b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8017fa6f1241674a82c7614c160a66ad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43d8753312614fe9206468bac5da5e12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebc6a8f668045d282ab958fd72cba79f |
publicationDate | 2021-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-202104088-A |
titleOfInvention | Ytterbium-doped barium zirconate particles and mehtod for producing same |
abstract | According to the present invention, there is provided a method for producing ytterbium-added barium zirconate particles represented by the composition formula (I) BaZr1-xYbxO3-[delta] (wherein x is a number satisfying 0.1 ≤ x ≤ 0.6, and [delta] represents the oxygen deficiency amount), the method contains: (a) a step of mixing a seed crystal of barium hydroxide, zirconium hydroxide, ytterbium hydroxide and ytterbium-added barium zirconate with water to obtain a first slurry; (b) a step of wet-milling the first slurry to obtain a second slurry containing particulate solid matter having an average particle size of 3.0 [mu]m or less; (c) a step of adding barium hydroxide to the second slurry to obtain a third slurry; (d) a step of hydrothermally reacting the third slurry to obtain a fourth slurry; and (e) a step of removing excess barium hydroxide by washing the fourth slurry with water after acid treatment; at that time, the Ba/(Zr+Yb) molar ratio of the slurries in the step (a) and the step (c) is set within a predetermined range. According to the present invention, it is possible to obtain ytterbium-added barium zirconate particles having a uniform composition, which does not include a heterogeneous phase, and which are fine and highly crystalline, by a liquid phase method suitable for industrial mass production at low cost. |