http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-202100647-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09F9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K59-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-375 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K19-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-14 |
filingDate | 2020-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cda7edd30854ea16c54cafabd6a0832 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50e444a862c1dfc847d1c7842971c9cd |
publicationDate | 2021-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-202100647-A |
titleOfInvention | Polymerizable liquid crystal composition, liquid crystal cured film, elliptical polarizing plate and organic EL display device |
abstract | The object of the present invention is to provide a polymerizable liquid crystal composition, which is suitable for forming and exhibiting high optical properties, and can suppress the optical properties even under severe conditions such as high temperature and high humidity or under conditions such as exposure to sunlight. A liquid crystal cured film with excellent durability and decreased characteristics over time. A polymerizable liquid crystal composition containing a polymerizable liquid crystal compound, a primary antioxidant, and a photopolymerization initiator. The polymerizable liquid crystal compound has an ester structure and a (meth)acrylic acid group, and has a wavelength of 300 to 400 A polymerizable liquid crystal compound exhibiting maximum absorption at nm, and the photopolymerization initiator is a compound having a sulfide structure represented by the following formula (I): [In formula (I), A 1 and A 2 each independently represent a hydrogen atom, an aliphatic hydrocarbon group having 1 to 25 carbon atoms which may have a substituent, an alicyclic group having 3 to 25 carbon atoms which may have a substituent, Or an aromatic group with 6 to 25 carbons that may have a substituent, and -CH 2 -contained in the aliphatic hydrocarbon group, the alicyclic group, and the aromatic group may be substituted with -O-, -CO- , -C(=N)O-, -SO 2 -or -S-, the carbon atoms constituting the aromatic group can be substituted with oxygen, sulfur or nitrogen], the molecular weight of the above-mentioned primary antioxidant is 150 g /mol above. |
priorityDate | 2019-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |