abstract |
The particles of the liquid crystal polyester resin composition of the present invention are characterized by comprising a liquid crystal polyester resin (A) and an inorganic filler (B). The particles contain voids having an equivalent spherical diameter of 10 μm or more and 1000 μm or less. In the total amount, the existence rate of voids with an equivalent spherical diameter of less than 400μm is 40% to 90%, the length is 1mm to 5mm, and the maximum diameter is 1mm to 3mm. The average of the aforementioned voids per particle The number is 4 or more and 9 or less. |