abstract |
The present invention provides a rayon fiber with fibrillation tending to be improved. It requires less than 80 minutes to obtain a 50 ° SR value according to ISO 5267-1: 1999, and the working capacity [cN / tex] *%] Is less than 50%, and a method for producing the fiber and a product containing the fiber. |