Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-122 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-124 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2451-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2433-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2467-006 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-385 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-255 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-30 |
filingDate |
2018-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1ec8455982406340626777514bb5334 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a382c2d8742cc28614d4cdaf3e32a596 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec31f8f98f00ff4934a6d0eae47f633c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0cd6ac95d16d0f427680d57003899a7 |
publicationDate |
2019-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201923006-A |
titleOfInvention |
Adhesive sheet |
abstract |
The present invention provides an adhesive sheet which can maintain secondary workability even after being applied to a temperature of about 50 ° C at the initial stage of adhering to the adherend, and then the adhesive force is greatly increased. The present invention provides an adhesive sheet comprising an adhesive layer. The pressure-sensitive adhesive layer contains a polymer A and a polymer B as a copolymer of a monomer having a polyorganosiloxane chain and a (meth)acrylic monomer. The glass transition temperature T m1 of the polymer B based on the composition of the (meth)acrylic monomer is 50° C. or higher and 100° C. or lower. After the adhesive sheet was heated at 80 ° C for 5 minutes after the attachment, the adhesive force N 80 was 5 times or more of the adhesive force N 50 after being left at 50 ° C for 30 minutes after the attachment. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113861896-A |
priorityDate |
2017-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |