abstract |
A hard-coated film comprising a base film made of a thermoplastic resin containing an alicyclic structure-containing polymer and a hard coat layer provided on at least one side of the base film, on the hard coat layer, pressed When the steel wool with a diameter of 13mm and a load of 500gf was applied to the hard coat, the number of scratches on the hard coat was less than 5 when the round was repeated 10 times. Before the light resistance test of the hard coat irradiated with ultraviolet light for 48 hours, the hard The coating is scored to form 100 areas with a size of 1 mm × 1 mm. When the cellophane tape is attached to the aforementioned 100 areas and peeled off within 1 second, the number of areas of the aforementioned hard coat layer remaining R1 is 90 or more, and after the light resistance test, the number R2 of the areas of the hard coat layer remaining is 90 or more. |