http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201903008-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 |
filingDate | 2018-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29cbfb6cd3cbc5fcb5ceecfb0fdbac60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_716f97c220666b8b0a024a8a88591c84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_715d4e595ffb07ff0d32a684e72b0011 |
publicationDate | 2019-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201903008-A |
titleOfInvention | film |
abstract | A film comprising a substrate layer and a sealing layer and having a thickness of 20 μm or more and 150 μm or less, and wherein one surface layer of the film is a substrate layer and the other surface layer is a sealing layer film, wherein the sealing layer It contains a resin composition and has a thickness of 5 μm or more and 100 μm or less. The crystallization index [D730 / D720] of the surface of the sealing layer on the film surface measured by the multiple reflection ATR-IR method is 0.680 or more and 0.900 or less. In a state where the sealing layer on the surface of the film is in contact with the following adherend (X), the film is heated on the adherend (X) described below under the conditions of a temperature of 160 ° C., a time of 1 second, a width of the sealing rod of 10 mm, and a pressure of 450 kPa. At the time of sealing, the ratio of the thickness of the resin composition of the sealing layer that is eluted from the heat-sealed portion to the non-heat-sealed portion and solidified to the thickness of the non-heat-sealed portion of the sealing layer is 1.80 to 2.20. Adhesion (X): Thickness of impact-resistant polystyrene with a melt flow rate of 3.0 g / 10 minutes or more and 4.0 g / 10 minutes or less and a Ficca softening temperature of 95 ° C or more and 100 ° C or less It is an adherend of 350 μm or more and 550 μm or less. |
priorityDate | 2017-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |