Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5128cfc84a0fb189fceb3cd240c44493 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2800-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F287-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F287-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 |
filingDate |
2018-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e5b9e2562d01cf82d95b9adf53f4619 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3fadc9bd5dbffbcc91feb5fe39bb2311 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c5f76110d31de8fd3c6014f08e494982 |
publicationDate |
2019-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201900691-A |
titleOfInvention |
Modified block copolymer, method for producing modified block copolymer, and resin composition |
abstract |
The modified block copolymer of the present invention includes a polymer block (A) mainly composed of a vinyl aromatic compound, a polymer block (B) mainly composed of a conjugated diene compound, and NHx (x = 0 ~ 2) atomic group (C). In the modified block copolymer, the polymer block (B) mainly composed of a conjugated diene compound is a hydride, and the atomic group (C) having NHx (x = 0 to 2) is contained in a side chain And the compound forming the atomic group (C) having NHx (x = 0 to 2) satisfies the following conditions. Condition: When the compound forming the above-mentioned atomic group (C) having NHx (x = 0 to 2) is reacted with the maleic anhydride-modified group in the maleic anhydride-modified block copolymer, The MFR value of the modified block copolymer at 230 ° C and a load of 2.16 kg becomes more than 0.1 times the MFR value of the maleic anhydride modified block copolymer at 230 ° C and a load of 2.16 kg. |