abstract |
The polyamidoamine resin composition of the present invention contains a semi-aromatic polyamidoamine (A), an aliphatic polyamidoamine (B) having a melting point of 280 to 320 ° C, and 5 to 30% by mass of a phosphinic acid metal salt ( C), 5 to 60 mass% of reinforcing material (D), 0.1 to 8 mass% of metal carbonate (E), and 0.01 to 3 mass% of fatty acid barium salt (F); (A) and (B) The total content is 30 to 85% by mass, and the mass ratio (A / B) of (A) to (B) is 90/10 to 40/60. |