abstract |
The glass container described herein has at least two performance attributes selected from the group consisting of delamination resistance, improved strength, and improved damage resistance. In one embodiment, the glass container may include a body having an inner surface, an outer surface, and a wall thickness, the wall thickness extending between the outer surface and the inner surface. At least the inner surface of the main body may have a delamination factor of 10 or less. A tough inorganic coating can be positioned around at least a portion of the outer surface of the body. The outer surface of the body having the tough inorganic coating may have a friction coefficient of less than or equal to 0.7. |