http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201805330-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_696ca0ae93d5cf5a686273601361781f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-30 |
filingDate | 2017-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e2807a580122bbba4a7d41b1c819571 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d8cf79bc440d55eeaae27b7fbbf270f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_672726e5107ae576e7512047cbe51e93 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0278d81d1d1c4b5e61f2d3ad39f5fae9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f60f75f9e2126837a26532f89de4c397 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_afaf5778bc05e21b28a66de6c101ccfe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_345fc3dad04e7b5aa70c3ed3a2b9dad7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86092f911512b48b88e9b82a1a464427 |
publicationDate | 2018-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201805330-A |
titleOfInvention | Method for producing high molecular weight aromatic polycarbonate resin |
abstract | The present invention provides a method for producing a high-molecular-weight aromatic polycarbonate resin that has excellent fluidity, can achieve a good hue, and has sufficient molecular weight.nn n n A method for producing a high-molecular-weight aromatic polycarbonate resin, comprising the steps of: mixing a diol compound represented by the general formula (1) with a catalyst to obtain a catalyst composition; and using the obtained catalyst composition to The molten state is maintained, and a step of obtaining a prepolymer mixture by mixing with an aromatic polycarbonate prepolymer within 10 hours after the catalyst composition is obtained; and heating the obtained prepolymer mixture under reduced pressure to obtain a high Polymerization step of molecular weight aromatic polycarbonate resin.nn n n n n n n n n n In the formula (1), R 1 to R 4 each independently represent a hydrogen atom, a halogen atom, or a linear or branched alkyl group having 1 to 5 carbon atoms, and Q represents a group selected from an aliphatic hydrocarbon group, an aromatic hydrocarbon group, an oxygen atom, A divalent group or a single bond which may have a substituent and is composed of at least one of the group consisting of a sulfur atom, a sulfo group, a fluorenylene group, a carbonyl group, a dialkylsilyl group, and a diarylsilyl group. |