abstract |
The present invention provides a transparent sintered body having few defects derived from bubbles. A method for producing a ceramic molded article, comprising at least a ceramic having a quotient of a loose bulk density and a tapped bulk density, that is, a Hausner ratio exceeding 1.0 and 1.2 or less The step of subjecting the particles to press forming. And a method for producing a transparent sintered body, comprising at least the steps of the above-described production method for obtaining a ceramic molded article, and the step of heating and sintering the obtained ceramic molded article to obtain a transparent sintered body, wherein the transparent sintered body is A linear transmittance of 78% or more in a wavelength other than the characteristic absorption of an element, which is a wavelength of 600 nm or more and 2000 nm or less. |