http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201739833-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K19-544 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1339 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3417 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1339 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-375 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
filingDate | 2017-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87de9d634ce66f5e7ba30091e565e1e4 |
publicationDate | 2017-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201739833-A |
titleOfInvention | Light-shielding sealant for liquid crystal display element, upper and lower conductive materials, and liquid crystal display element |
abstract | An object of the present invention is to provide a light-shielding sealant for a liquid crystal display element which is excellent in curability and storage stability and which can suppress liquid crystal contamination. Moreover, an object of the present invention is to provide an upper and lower conductive material and a liquid crystal display element using the light-shielding sealant for a liquid crystal display element. The present invention relates to a light-shielding sealant for a liquid crystal display element comprising a curable resin, a photoradical polymerization initiator, an amine adduct compound, and an opacifier, and the wavelength of the above photoradical polymerization initiator The light absorption coefficient at 365 nm was 5000 mL/g‧cm or more, and the absorbance at 365 nm was measured in acetonitrile obtained by mixing the photoradical polymerization initiator at a concentration of 0.1 mg/mL. |