http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201739786-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_98ec0629c8a506ce664ac51ffe289487 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-79 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate | 2017-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bbdba0dcfade3b9a0140d5f050a6d7b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b015f67a145d70a0448bef3521cdef9d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c87641943e4e54ccbcbfbdfdb48d315 |
publicationDate | 2017-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201739786-A |
titleOfInvention | Full aromatic liquid crystal polyester resin and its manufacturing method |
abstract | An object of the present invention is to provide a wholly aromatic liquid crystal polyester resin which has high mechanical strength, excellent filling property, and foaming resistance and low warpage. The wholly aromatic liquid crystal polyester resin of the present invention is characterized in that it comprises the structural units (I) to (V) represented by the following formulas (I) to (V), and the above aromatic liquid crystal polyester The composition ratio (mol%) of the structural units (I) to (V) in the following conditions satisfies the following conditions: 15 mol% ≦ structural unit (I) ≦ 35 mol% 5 mol % ≦ structural unit (II) ≦ 15 mol % 21 mol % ≦ structural unit (III) ≦ 29 mol % 1 mol % ≦ structural unit (IV) ≦ 9 mol % 25 mol % ≦ structural unit (V) ≦ 40 mol % structure Unit (I) + structural unit (II) + structural unit (III) + structural unit (IV) + structural unit (V) = 100 mol%, and the melting point of the above wholly aromatic liquid crystal polyester resin is 320 ° C or higher. |