abstract |
The aqueous resin composition for a touch panel of the present invention has a refractive index of 1.60 or more and contains a water-soluble crosslinking agent having at least two polymerizable functional groups, and is formed by using an aqueous resin composition for a touch panel at 23 ° C. When it is a 5 mass% aqueous solution, the surface tension is 40 mN/m or less. |