Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-558 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2571-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2221-6834 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2221-68327 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-51 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-6836 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-30 |
filingDate |
2014-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11b6bac084a77732dfb5d748990acda5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_487cc7d567c4004516b9aa19a2545921 |
publicationDate |
2015-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201505836-A |
titleOfInvention |
Stress relaxation film, laminate, surface protection film for semiconductor, method for manufacturing semiconductor device, and resin modifier |
abstract |
A stress-relieving film comprising: a thermoplastic resin A comprising 70 mol% to 90 mol% of a structural unit derived from 4-methyl-1-pentene, and 10 mol% to 30 mol% of a carbon number of 2 Or a structural unit of an α-olefin of 3, and a copolymer derived from a structural unit of an α-olefin having 4 to 20 carbon atoms other than 4-methyl-1-pentene, wherein the ratio is 10 mol% or less; The thermoplastic resin B other than the thermoplastic resin A is at least 1 selected from the group consisting of a vinyl polymer, a propylene polymer, a butene polymer, and a 4-methyl-1-pentene polymer. The content of the thermoplastic resin A is 50% by mass to 98% by mass based on the total mass, and the content of the thermoplastic resin B is 2% by mass to 50% by mass based on the total mass. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I746829-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114651044-A |
priorityDate |
2013-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |