http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201504175-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44ff3005508304394801e265e503b811 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B5-193 |
filingDate | 2014-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec17986000a0b549a514963f49a48e20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61c8f31cb7120386ccfcdf2d19327f09 |
publicationDate | 2015-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201504175-A |
titleOfInvention | Glass, broken glass, and manufacturing method of optical element |
abstract | The present invention provides a method for producing glass, a method for producing cullet and an optical element, which is produced by a rough-melt-remelting method, which is excellent in clarity, and has good glass properties (homogeneity, transmittance, etc.) and can be lowered. Environmental load and production costs. The method for producing a glass according to the present invention includes: a rough melting step of melting a preparation material to obtain cullet; and a remelting step of remelting the cullet to obtain a glass, wherein the rough melting step and the In at least one of the remelting steps, at least one of a treatment of bubbling a gas containing carbon dioxide in the molten material and a treatment of adding carbon dioxide to the molten atmosphere is performed. |
priorityDate | 2013-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |