abstract |
A pressure-sensitive adhesive comprising at least two constituent components each constituting a phase, and the constituents constitute an IPN having at least two phases via a cross-linking built-up reaction, in particular Wherein the first phase (elastomer phase) has a softening temperature of at least less than 23 ° C depending on the DSC, and the second phase has a softening temperature of greater than 23 ° C depending on the DSC after the synthesis reaction, wherein the second phase has crosslinks after the synthesis reaction The shape of the nanoparticle network. |