Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee1c19da359446fb5c4f0458a57b783d |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C21-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C4-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B27-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01J3-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-076 |
filingDate |
2013-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d23d5e8659e128d1739903ed5cd6459d |
publicationDate |
2014-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201412653-A |
titleOfInvention |
Glass manufacturing method, chemically strengthened glass (1) |
abstract |
The present invention provides a method for producing a glass having high strength and obtaining a desired color tone, and a chemically strengthened glass. A method for producing a glass, characterized in that after the glass containing the coloring component is subjected to a chemical strengthening treatment, the temperature region from the chemical strengthening treatment temperature to 300 ° C is cooled at a cooling rate of 30 ° C /min or more. |