abstract |
The present invention provides a laminate which is thin and lightweight, is excellent in gas barrier properties, flexibility, and durability, and is excellent in flatness. The present invention relates to a glass plate fluororesin laminate having a glass plate having a thickness of 10 to 500 μm and a fluororesin coating layer having a thickness of preferably 0.1 to 1,000 μm. In particular, the ratio of the thickness of the glass plate to the fluororesin coating layer is preferably 0.001 to 10 in terms of the fluororesin coating layer/glass plate. Further, the transmittance at a wavelength of 400 to 700 nm is preferably 80% or more. Further, the laminate is preferably used as a protective sheet. Further, the laminate is preferably applied to a photoelectric conversion element. |