http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201404467-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_955b31616eeb6aba94e350fdd51fb516 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0205 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07D301-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-688 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0213 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07D301-10 |
filingDate | 2013-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_38c0206fa63c6e69e922e108839b682d |
publicationDate | 2014-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201404467-A |
titleOfInvention | Method for producing manganese catalyst supported by manganese |
abstract | The present invention provides a method of making a manganese catalyst-supported silver catalyst intermediate. The method includes preparing a first solution comprising a manganese component and a binder and combining it with a second solution comprising silver to form an impregnation solution. The pH of the first solution is less than or equal to 7 at any time during or after the preparation of the first solution. The support is then impregnated with at least a portion of the impregnation solution to form the catalyst intermediate. The pH of the impregnation solution is greater than 7. |