http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201400519-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_696ca0ae93d5cf5a686273601361781f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3855 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7642 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G75-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3876 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3868 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-3475 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3874 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-053 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-38 |
filingDate | 2013-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_38a2d36cf636af83210907c0c886fb0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75e8a2af0d72dbec1e23186252a60ee9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4059b941b849f42d38970ce99448cfad |
publicationDate | 2014-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201400519-A |
titleOfInvention | Optical material manufacturing method |
abstract | The present invention provides a method for blending, which comprises a method for producing an optical material of a predetermined (a) compound, (b) compound, (c) compound, (d) compound, and (e) compound, which can suppress mold release marks. Residual adverse conditions occur. In the present invention, the defects remaining in the release mark are suppressed by the following first steps to the fifth step. First step: a step of dissolving the compound (b) in the compound (a) to obtain a first liquid. Second step: a step (e) is added to the first liquid obtained in the first step and mixed to obtain a second liquid containing no (d) compound. The third step: a step of adding the compound (c) to the second liquid obtained in the second step to obtain a reaction mixture. Step 4: a step of adding the compound (d) to the reaction mixture obtained in the third step and mixing them to obtain a resin composition for an optical material. The fifth step: a step of casting the resin composition for an optical material obtained in the fourth step and polymerizing it to obtain an optical material. |