Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2203-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T156-1972 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T156-1189 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-318 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S156-937 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S156-924 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133331 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-0073 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09F9-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13 |
filingDate |
2013-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7c00a67f0a58f5f5488e98581346ea9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8c18a3fa59b3e421950fab7065b2998 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ef980218291f206996de07feb24fff9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d846f84293e00fa37f033be6556efc8 |
publicationDate |
2013-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201348796-A |
titleOfInvention |
Flat panel display manufacturing method |
abstract |
The present invention provides a method of manufacturing a flat panel display having an optical laminate on a display surface side in which two optical elements are bonded to each other through an adhesive sheet or a curable resin layer, the method comprising the following steps 1 to 4, or steps 1 to 5, and allow at least one of the optical elements to be used as the optical element in step 1 after step 4 or step 5: step 1: through the adhesive sheet or curable Step of Resin Layer Bonding Two Optics to Each Other and Applying Autoclave Treatment to Provide Optical Laminate Step 2: Checking the Appearance of the Optical Laminate Obtained in Step 1 Step 3: Using the Optical Layer Checked by Step 2 Step 4 of assembling the flat panel display by the pressure plate Step 4: Separating the two optical elements in the optical laminate rejected by the step 2 by the relative rotation of the two optical elements through the opposite perpendicular lines as the rotation axis : the step of cleaning the optical component obtained in step 4. |