Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bb4ee28d43b5e8d4a3c5141fa9bcfeb0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D2518-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2483-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2327-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-0427 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 |
filingDate |
2013-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23d339c9f2ffabb078efdb90168a73de http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63cddf6a6632764ed7f3bd0b44a6adcc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b500f933fc55782b812d219b43384bb5 |
publicationDate |
2013-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201343817-A |
titleOfInvention |
Method for producing article having fluorine-containing decane-based coating film |
abstract |
The present invention provides a method of making an article comprising a substrate and a perfluoropolyether-containing decane-based coating film coated on the surface of the substrate, wherein the method comprises forming a perfluoropolyether having enhanced friction durability A group of decane-based coating films. The method comprises the steps of: (a) forming a pre-coating film comprising a perfluoropolyether group-containing decane compound having a hydrolyzable group bonded to Si on a surface of the substrate; (b) supplying moisture to the pre-existing The film is coated; then (c) a film is coated before heating the surface of the substrate in a dry atmosphere exceeding 60 ° C to form a perfluoropolyether group-containing decane-based coating film derived from the pre-coat film. |