Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2baf849d216e689ecc40ccc931a7a7bc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133715 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-123 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-0254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-303 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133788 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133711 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133715 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1337 |
filingDate |
2012-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60cae6bd3958ba4a0dad6a04eaea01bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05290110d78dcb80f020528b5ce27574 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_84c1bdc02a3ae9cbbf54dd2e5e844c21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cfe9c16c4fc32ec480eac177d090290d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_481e175c24265e084486dd1b88c2c5e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_faa89128c2ea24b30b47490d1314cc2f |
publicationDate |
2013-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201341413-A |
titleOfInvention |
Method for manufacturing liquid crystal alignment film, liquid crystal alignment film and liquid crystal display element |
abstract |
The present invention provides a method for producing an anisotropic liquid crystal alignment film which can be introduced into a film without friction and high efficiency, and provides a liquid crystal alignment film and a liquid crystal display element. A method for producing a liquid crystal alignment film, which is a method for producing a liquid crystal alignment film having the steps [I] to [III]; [I] forming a side chain type high in liquid crystallinity on a substrate at a specific temperature range a step of molecular film, [II] a step of irradiating the polarized ultraviolet light to the side chain type polymer film, and [III] a step of heating the ultraviolet light-irradiated side chain type polymer film, which is characterized by [II] step The ultraviolet irradiation amount is in the range of 1% to 70% of the ultraviolet irradiation amount when the ΔA of the side chain type polymer film is the maximum, and the ΔA is ultraviolet rays parallel to the polarization direction of the polarized ultraviolet light. The difference between the absorbance and the UV absorbance in the vertical direction. |