Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-0002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0094 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2007-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-3406 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2063-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2509-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0013 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-24 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-46 |
filingDate |
2013-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f631d95e38634634cd9186f946dc6b19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13c1250b43b502620689d4e9881ac9e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_469890dbe6fae31111831c62edd4c2cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f8508eab0730e2b0d5100fb0fd8cc46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dba61f510fb3b950a8ae414ae6295525 |
publicationDate |
2013-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201336662-A |
titleOfInvention |
Thermal conductive sheet manufacturing method |
abstract |
An object of the present invention is to provide a method for producing a thermally conductive sheet which can effectively reduce the void ratio and the thermal conductivity in the plane direction while effectively preventing the breakage of the plate-shaped boron nitride particles. And a thermal conductive sheet excellent in softness. In the method of producing the thermally conductive sheet 100, the raw material component 27 containing the plate-shaped boron nitride particles 23 and the polymer matrix 24 is prepared, and the long sheet 20 is formed from the raw material component 27 by the calender 1, and the strip is formed. The sheet 20 is pressed. |