Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-92714 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-0079 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-022 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-911 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-288 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B13-04 |
filingDate |
2012-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73790757fbb575fa9113b289f435d8f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_15d254d5aa4eee613a8e1f45c30ef999 |
publicationDate |
2013-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201335246-A |
titleOfInvention |
Method for producing liquid crystal polymer composition and formed body |
abstract |
The present invention relates to a method for producing a liquid crystal polymer composition, comprising: using a melt kneading extruder including a nozzle, a cylinder, and a screw provided in the cylinder, and a component provided at a supply port of the cylinder (A) a magnetic filler obtained by heat-treating a composite material composed of a liquid crystal polymer and a component (B) ceramic powder and soft magnetic metal powder in an inert gas atmosphere, and supplying the magnetic filler to the cylinder, and the component (A) and the component (A) The component (B) is melt-kneaded to obtain a kneaded product; the kneaded product is extruded outside the melt kneading extruder by the nozzle; and the kneaded product is cooled at a cooling rate of 60 ° C /sec or less. And a molded body obtained by molding the liquid crystal polymer composition obtained by the production method. |