abstract |
An object of the present invention is to provide a slurry composition obtained by which the obtained ceramic green sheet has sufficient mechanical strength, has little dimensional change during storage, and is less likely to cause interlayer peeling at the initial stage of degreasing. The solution of the present invention is a slurry composition comprising a polyvinyl acetal resin, 2-methylpropionic acid and an organic solvent, wherein the polyvinyl acetal resin has a polymerization degree of 500 or more and 6000 or less, and a vinyl ester unit content. It is 0.01~30 mol%, the degree of acetalization is 50-83 mol%, and has a chemical formula of 30% or more in the molecule relative to the total molar amount of all acetalized structural units (1) The structural unit is shown; wherein the 2-methylpropionic acid is 10 to 1000 ppm based on the polyethylene acetal resin. |