http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201314281-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 |
filingDate | 2012-09-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_238da4b445adba493a3a7925af73e586 |
publicationDate | 2013-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201314281-A |
titleOfInvention | Polarizing plate, manufacturing method thereof and liquid crystal display device |
abstract | A method for producing a polarizing plate capable of producing a polarizing plate having less unevenness in display when incorporated in a liquid crystal display device at a low manufacturing cost, comprising: a deuterated cellulose having a total thiol substitution degree of 2.7 to 3.0 a step of saponification treatment of the first deuterated cellulose film; a second deuterated cellulose film containing deuterated cellulose having a sugar ester compound and a mercapto degree of substitution of 1.5 to 2.6 at a temperature of Tg-20 ° C or higher a step of performing heating; a step of saponifying the second deuterated cellulose film under the same conditions as the saponification conditions of the first deuterated cellulose film; and the above saponification using the first deuterated cellulose film The step of holding the polarizer on the treated surface and the saponified surface of the second deuterated cellulose film. |