http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201249925-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C67-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C67-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31786 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K19-3809 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate | 2012-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_220739ca1731001f4373cdc24e1b37ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_42ba6d48dcc08619802519bdfabe37e5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4c7a6fc12f51911e1b57f8d4c016ab1 |
publicationDate | 2012-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201249925-A |
titleOfInvention | Method for producing liquid crystal polyester |
abstract | Disclosed is a method for producing a liquid crystal polyester, which includes the steps of: (1) polycondensing a mixture of 70.5 to 71.5 mol% of a compound represented by the defined formula (I) (for example, 4-acetoxybenzoic acid) with 28.5 to 29.5 mol% of a compound represented by the defined formula (II) (for example, 6-acetoxy-2-naphthoic acid) to form a prepolymer, wherein the prepolymer has a flow initiation temperature of 200 DEG C or higher, and the mixture is polycondensed until reaching the temperature which is at least 30 DEG C lower than the polycondensation temperature; (2) removing the prepolymer in a molten state, followed by solidification and further grinding to produce prepolymer particles; and (3) subjecting the prepolymer particles to a heat treatment at 200 to 310 DEG C under circulation of an inert gas while remaining in a solid phase state. |