http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201220339-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2bb79367ec64b8bd089c3e72449bad58 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T29-4911 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T29-49115 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2220-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0404 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-0029 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G13-04 |
filingDate | 2011-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dd2e1ef54cefa7571ebf39402b4920c |
publicationDate | 2012-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201220339-A |
titleOfInvention | Method for drying pair of electrodes, method for producing lithium-ion rechargable battery, method for producing electric double-layer capacitor, and method for producing lithium-ion capacitor |
abstract | This method for drying an electrode pair includes: a step in which a collector is coated with a positive-electrode material, yielding a positive electrode; a step in which a collector is coated with a negative-electrode material, yielding a negative electrode; a step in which an electrode pair (7) is produced, said electrode pair comprising one or more sets of the aforementioned positive electrode and negative electrode laminated together with a separator or separators interposed therebetween; and a step in which said electrode pair (7) is placed inside a container. Said method also includes at least one of the following drying steps: a step in which the positive electrode and/or the negative electrode is dried using a freeze-drying method; and a step in which the container containing the electrode pair is dried using a freeze-drying method. This makes it possible to provide a method for manufacturing a lithium-ion secondary battery, a method for manufacturing an electric double-layer capacitor, a method for manufacturing a lithium-ion capacitor, and a method for drying an electrode pair whereby the time it takes to dry said electrode pair can be reduced without causing defects such as wrinkles in the separator(s). |