http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201210979-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a6df5a19802a9643e0160c187d17667b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B12-00 |
filingDate | 2010-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_259bd8ca560f56fa30df9dc75effbfbf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae44a9dc31bb9f4b3da0da8ad032ce4e |
publicationDate | 2012-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201210979-A |
titleOfInvention | Alkali activation slurry |
abstract | The present invention provides an alkali activation slurry for concrete, comprising alkali activation solution and inorganic powder, wherein the molar ratio of the silicon dioxide in the alkali activation solution to the alkali metal oxide is in the range of 0.25 to 0.5, and the molar ratio of silicon dioxide to aluminum oxide is in the range of 20 to 100. The alkali activation slurry not only can be independently used as reinforcement material or fireproof material, but also can form sand slurry or concrete to replace cement slurry to be construction material by adding a proper amount of rough and fine aggregates. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111302682-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I596076-B |
priorityDate | 2010-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.