http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201209118-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_962adbf7d50e742218f3d536a63df612 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-318 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J175-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-385 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-22 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 |
filingDate | 2011-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03875c0fc93f0e3e66f507e86b8b75fe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59906fb06d817c15dfe03e99360575d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_456184c0c1b5147f3558cb709eb9b558 |
publicationDate | 2012-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201209118-A |
titleOfInvention | Adhesive composition, adhesive agent and adhesive sheet |
abstract | The subject of the present invention is to provide an adhesive composition having both excellent light leakage resistance and durability when used in optical components such as polarizers, and also to provide a preparation method of the same, an adhesive agent and an adhesive sheet. The solution of this invention is an adhesive composition which comprises: a first (meth)acrylate polymer (A) having a weight average molecular weight of 700,000 to 2,500,000; a second (meth)acrylate polymer (B) having a weight average molecular weight of 8,000 to 250,000; and a cross-linking agent (C). The ratio of the second (meth)acrylate polymer (B) to 100 parts by weight of the first (meth)acrylate polymer (A) is 5 to 40 parts by weight. The second (meth)acrylate polymer (B) contains a monomer, having a functional group (b1) to react with the cross-linking agent (C), as a component and has a ratio of the monomer of said functional group (b1) being more than 1 mass% and less than 50 mass% in the second (meth)acrylate polymer (B). The functional group contained in the second (meth)acrylate polymer (B) to react with the cross-linking agent (C) in general contains only the functional group (b1). The first (meth)acrylate polymer (A) does not contain a monomer having the functional groups capable of reacting with the cross-linking agent (C) as a component, or contains a monomer having a functional group (a1) that shows less reactivity with the cross-linking agent (C) than the functional group (b1) of the second (meth)acrylate polymer (B) as a component. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I648364-B |
priorityDate | 2010-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 105.