Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2848 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133528 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2835 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2891 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3033 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate |
2011-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3da7115ee4662f0b80d3ee5eb7ccb181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03cb7096f66d07956cece0789d14677b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4661976a16b2ae37502dff7dac60e02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4acbfeaeaae0a9abb05888f9f3819c2b |
publicationDate |
2012-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-201207062-A |
titleOfInvention |
Pressure-sensitive adhesive layer for optical films, pressure-sensitive optical film and image display device |
abstract |
The disclosed pressure-sensitive adhesive layer for optical films is formed by coating an aqueous pressure-sensitive adhesive dispersion comprising an emulsion of a (meth)acrylate polymer obtained by emulsion-polymerizing a monomer mixture containing a (meth)acrylate alkyl ester with C1-3 alkyl groups (a1) or alkoxysilyl group-containing monomer (a2) as well as a (meth)acrylate alkyl ester with C4-14 alkyl groups (b) in water in the presence of reactive surfactant and a radical polymerization initiator and then drying. The proportion of said reactive surfactant is 0.3 to 3 parts by weight with respect to 100 parts by weight of the monomer mixture and the saturated water absorption is 1.2 to 3.2 weight%. Even when the optical film on the side that the pressure-sensitive layer is to be laminated is formed from a material of low moisture permeability, said pressure-sensitive adhesive layer for optical films is able to exhibit heat durability in high temperature environments and is able to exhibit moisture durability in high humidity environments. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I636114-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I629518-B |
priorityDate |
2010-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |