http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201132819-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_49f5a779eff1897763fbeb8273e8ab99 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 2010-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2dee4cdb53ea8cb2f1e49a30241a9b2a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_25aa55ea1cc023a552f1a2e9707270bc |
publicationDate | 2011-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201132819-A |
titleOfInvention | Method to increase whiteness recycling of PET fibers and core-sheath type PET fibers manufactured by the same |
abstract | The method to increase whiteness recycling of PET (Polyethylene Terephthalate) fibers is to proceed spinning of the compositions formed of recycled PET (Polyethylene Terephthalate) with degree of whiteness hue between 55-80 and PET (Polyethylene Terephthalate) with degree of whiteness hue between 85-95 by a composite fiber spinning machine, thereby producing a core-sheath type PET (Polyethylene Terephthalate) fiber, wherein the core layer is formed by the recycled PET (Polyethylene Terephthalate), the sheath layer is formed of the compositions, and the cross section of the fiber is a concentric circle, the relation between the radius R1 of the inner circle and the radius R2 of the outer circle in the concentric circle is as the following formula (I) : 1.11≤R2/R1≤4.48 (I). |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I773573-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11766835-B2 |
priorityDate | 2010-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 19.