http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-201131194-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6a162b65402a9a79580e3ae31dcbf3fa |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133502 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-116 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 |
filingDate | 2010-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd778f5f770b0bc391ee4310d9ffed37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1bc92fae04c5fc84cf4e7d599ced1619 |
publicationDate | 2011-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-201131194-A |
titleOfInvention | Anti-reflection film and production method thereof |
abstract | With respect to anti-reflection film, there demands a low production cost anti-reflection film, further demands an anti-reflection film which excels in optical characteristics like anti-reflection ability or without interference irregularity, further demands high scratch-resistance for establishing on surface of display, further demands an anti-reflection film which has antistatic function for prevention of attachment of dusts. With respect to the present invention, there provides an anti-reflection film which is low at production costs, and has excellent optical characteristics and excellent scratch-resistance and antistatic function. To arrive at the present invention is an anti-reflection which laminates localized layer and low refractive index layer in this order on at least one side of transparent substrate, wherein the aforementioned localized layer localizes and laminates intermediate layer, hard coat layer, antistatic layer containing conductive materials, leveling layer containing leveling materials in this order at least from transparent substrate side. |