Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_097405822d505467fd50f7100022cd56 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J153-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J5-06 |
filingDate |
2008-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ed0efbe1beb8316a22a02511e94a813 |
publicationDate |
2009-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
TW-200927826-A |
titleOfInvention |
Saturated polyester resin composition and hot melt adhesive composition |
abstract |
Disclosed is a saturated polyester resin composition which is excellent in sealing properties and adhesive strength to metal materials such as copper and aluminum as well as resin materials such as polyethylene terephthalate. This saturated polyester resin composition is particularly improved in adhesive strength at low temperatures. Specifically, the saturated polyester resin composition contains a saturated polyester resin, a crystalline polyolefin resin and a thermoplastic soft acrylic resin. The saturated polyester resin composition may further contain an epoxy resin. The thermoplastic soft acrylic resin preferably has a Shore A hardness of less than 90 and a melt index at 190 DEG C under a load of 2.16 kg of not less than 10 g/10 minutes. |
priorityDate |
2007-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |