http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-200825223-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3597e746ed8bd1a07ac7eb3bfe5c8075 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-641 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-638 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-681 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-637 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H3-153 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H3-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-02 |
filingDate | 2006-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e6924525a738ec4e73db43edc4e1f2a9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3462e74c4cd5de56f5e93384be2b6dfc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b27e45872f6a5d16c737e53d7557a2d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7016574e156999bb5f812de3c58cbfe7 |
publicationDate | 2008-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-200825223-A |
titleOfInvention | Spunbond non-woven containing bamboo charcoal and method for fabricating the same |
abstract | A spunbond non-woven containing bamboo charcoal having functions of keeping warm, deodorization and noise elimination and including a plurality of non-woven fibers is described. The non-woven fibers include a bamboo charcoal mixture having bamboo charcoal and a polymer, wherein the bamboo charcoal has an amount of 0.05 to 35 wt% based on the total weight of the bamboo charcoal mixture. The present invention also provides a method of fabricating a single-compound or multi-compound spunbond non-woven containing bamboo charcoal. A bamboo charcoal grain containing bamboo charcoal is prepared, wherein the bamboo charcoal has an amount of 0.05 to 35 wt% based on the total weight of the bamboo charcoal grain. Next, the bamboo charcoal grain or the bamboo charcoal grain mixed with a polymer are spunbond with another polymer by using a spin apparatus to form a non-woven. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I551739-B |
priorityDate | 2006-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 65.