http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-200804521-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate | 2007-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0968de3d476d7c09d4ed9fa5474460bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a044fa871cee41cee92012094b96dd00 |
publicationDate | 2008-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | TW-200804521-A |
titleOfInvention | Polyorganosiloxane composition solidifiable under room temperature |
abstract | To provide a room temperature curable polyorganosiloxane composition having a low viscosity before curing and being excellent in physical properties of a cured product, particularly high elongation at break and high releasability from an adhered surface of a base material after curing. The room temperature curable polyorganosiloxane composition comprises 100 mass parts of (A) 5-95 mass% of a polyorganosiloxane sealed with trialkoxysilyl group at both terminals and (B) 95-5 mass% of a polyorganosiloxane sealed with dialkoxymonoorganosilyl group at both terminals, containing (C) 1-50 parts mass of one terminal trialkoxypolyorganosiloxane curing agent shown by general formula (1) (wherein R1, R2 and R3 represent a univalent saturated hydrocarbon group, X represents an oxygen atom or a bivalent hydrocarbon group and n represents an positive number giving viscosity of 0.005-100 Pa.s), (D) 1-50 parts mass of silica powder with specific surface area of 50 cm2/g or over and (E) 0.1-15 parts mass of a titanium chelate catalyst. |
priorityDate | 2006-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.