http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1752743-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_843cce7df8974af213595b986c6f05c5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 |
filingDate | 1989-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1992-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f0153bee1e86f4382009a4839b153c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0c0425bd5a8f4d09a478c83ddcfff1bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_962d4245af97604051c35a7a886a82de |
publicationDate | 1992-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1752743-A1 |
titleOfInvention | A method of making a polymeric material for coatings |
abstract | Use for sports coatings. The essence of the invention: prepare a rubber mixture by mixing (May hours) diene rubber 100 sulfur 1.8-3.3, vulcanization accelerator 1.5-2.3, zinc oxide 3-4, plasticizer 9-15, mineral filler 60-110 , stearin 1.0 to 4.5 antiactermel 1.0 to 5.6 pigment 4.0 to 5.0 and a modifying agent 0.8 to 6.0 As a modifying agent, use is made of termethanolamine, glycerin or applbenzyldimethylammonium chloride Mixture vulcanized, granulated. Mixed granular filler with polyurethane binder. Material curing Material characteristics Strength stretching 0.48-0.75 MPa, carries an elongation of 90- I5%, a change in tensile strength after irradiation with UV rays 78 - 89% of the original curing time 18-36 h, 2 tab (L C |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2649645-C2 |
priorityDate | 1989-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.