http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SU-1719344-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d82b3f07bf79a17ec1cd780c053a96bd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-00 |
filingDate | 1989-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1992-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e896483f94d0cf71136992740fded02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a0a1fe4fcd6f82e292630dbe1d2339e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c90047b46cf371f851953938d89841e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d7263caac6e14d26cf8bce087016e51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55d663dc005b3184591dea6534f1ea93 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3192e1965f2a77ee479dc140eee3cfd2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_497660627c7448e51c6235db30364f6e |
publicationDate | 1992-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | SU-1719344-A1 |
titleOfInvention | Raw stock for manufacturing heat insulating rock wool products |
abstract | The invention relates to the production of building materials and can be used for the manufacture of thermally insulating mineral wool products (1MBI) used in industrial and civil structures in order to increase the strength of the TM 8 I, reduce the gas output during their heat treatment and reduce the cost of products. The raw mix for the production of thermally insulated mineral wool products, including inorganic fiber (mineral wool), is a waste of a cured mineral wool carpet, a synthetic binder (phenol alcohol). foaming agent, water-repellent agent and water, additionally contains a water-soluble polyelectrolyte based on the bottoms of fiber production Nitron KO-1 (or KO-2) in the following ratio, wt.%: mineral wool 10.0 - 14.0; Waste of hardened mineral wool carpet 0.15 - 1.0; synthetic binder (phenol alcohol) 3t3 - 6.8; water-soluble polyelectrolyte based on the bottoms of the production of the fiber nitron KO-1 (or KO-2) 1.7 - 2.0; frother 0,1 - 0.2; water-repellent agent 0.5 - 1.0; water the rest. At a density of 231 - 250 kg / m, the compressive strength of products at 10% deformation is 1.47 - 1.70 kgf / cm, after sorption moisture - 1.26 - 1.48 kgf / cm. The content of organic substances is 5.2 - 7.4%. 1 tab. Yo |