Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_604954f531b7d40eccaa7118af8a290d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-04 |
filingDate |
1988-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1991-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f2525f93b038e058b3460477b8f9982 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cd31adc03ee23d7b0f3fae5f9eb921ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c5f13438863c8f32a05ef6b6f501ea7a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1eba31208eb16f7a3f646528a5b7296a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51dd0b426d557cc884b27bea957dfda9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f27c93048ea0621d938b901bdfda8273 |
publicationDate |
1991-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
SU-1685890-A1 |
titleOfInvention |
Raw mixture for manufacturing porous filler |
abstract |
The invention relates to the manufacture of building materials and can be used to make a porous aggregate from industrial waste. In order to reduce the bulk density of the aggregate, increase its strength and extend the swelling interval, the raw material mixture includes, mill%. sour cupola slag 77-87; sludge treatment plants 8-15; burned earth 5-8 The resulting aggregate has a bulk density of 150 kg / m3, strength 4.2-4.5 MPa, an expansion interval of 80-95 ° C. 2 tab. |